ASTM A335 P11 Pipe Bevel Ends With Caps
Mar 28, 2025
China ASTM A335 P11 Pipe Manufacurer GNEE Offers ASTM A335 P11 Pipe, 8IN X 20FT, SCH 80, Black Coating Surface Treatment, Bevel Ends With Caps.
.
ASTM A335 P11.
Size: 8 Inch X 20 Feet.
Wall thickness: SCH 80.