ASTM A 199 legirane čelične cijevi izmjenjivača topline

Oct 27, 2023

poređenje materijalaASTM A 199 cijev za izmjenjivanje topline

ASTM standard

Japanski

njemački

Britanski

JIS br

DIN tip

DIN br

BS br

BS razred

A199 T5

STBA25

 

12crmo19 5

3606

CFS625

A199 T11

STBA23

DIN17175

13crmo44

3606

CFS621

A199 T22

STBA24

SEW610

10crmo9 10

3606

CFS622

A199 t9

STBA26

DIN17175

12CrMo195

3606

 

Hemijska analiza ASTM A199 (%):

Kvalitet čelika

C

Mn

P

(maks.)

S

(maks.)

Si

Cr

Mo

ASTM A199 T4

0.15MAX

0.30-0.60

0.03

0.03

0.50-1.0

2.15-2.85

0.44-0.65

ASTM A199 T5

0.50-0.15

0.30-0.60

0.03

0.03

0.50MAX

4.00-6.00

0.45-0.65

ASTM A199 T9

0.15MAX

0.30-0.60

0.03

0.03

0.25-1.0

8.00-10.0

0.90-1.10

ASTM A199 T11

0.50-0.15

0.30-0.60

0.03

0.03

0.50-1.0

1.00-1.50

0.44-0.65

ASTM A199T22

0.50-0.15

0.30-0.60

0.03

0.03

0.50MAX

1.90-2.60

0.87-1.13

* Ni {{0}}.40 max; V 0.18-0.25; Cb 0.06-0.10; N 0.03-0.07; Al 0,04 max

Mehanička svojstva ASTM A199:

Kvalitet čelika

Vlačna čvrstoća (Mpa)

Granica tečenja (Mpa)

Izduženje

(%)

Tvrdoća HRB MAX

ASTM A199 T4

415MIN

170MIN

30/22

85HRB MAX

ASTM A199 T5

415MIN

170MIN

30/22

85HRB MAX

ASTM A199 T9

415MIN

170MIN

30/22

85HRB MAX

ASTM A199 T11

415MIN

170MIN

30/22

85HRB MAX

ASTM A199 T22

415MIN

170MIN

30/22

85HRB MAX